Medium-strength (40 MPa), compensated-shrinkage fibre-reinforced thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT T60 with 16.5-17.5 parts…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete.…
One-component, normal-setting cementitious mortar for smoothing concrete and cementitious render. TECHNICAL DATA: Maximum dimension of aggregate: 0.4 mm. Mixing ratio: 100 parts of MONOFINISH with…
One-component, normal-setting cementitious mortar for smoothing concrete and…