Two-component cementitious mortar with a low modulus of elasticity for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT BM comp. A with…
Two-component cementitious mortar with a low modulus of elasticity for…
Fibre-reinforced,
controlled-shrinkage mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT HI-FLOW E with 13-14 parts of…
Fibre-reinforced,
controlled-shrinkage mortar for repairing concrete. …
Hi-flow, compensated-shrinkage, steel fibre-reinforced, high-ductility cementitious mortar. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT HI-FLOW TI 20…
Two-component, thixotropic, fibre-reinforced, cementitious mortar with a low modulus of elasticity and added organic corrosion inhibitor for repairing concrete, applied in a single layer at a…
Two-component, thixotropic, fibre-reinforced, cementitious mortar with a low…
Quick-setting and hardening, compensated-shrinkage hi-flow mortar for repairing concrete and fixing drains, manholes and urban architectural fittings in place. TECHNICAL DATA: Maximum dimension of…
Quick-setting and hardening, compensated-shrinkage hi-flow mortar for repairing…
Hi-flow, steel fibre-reinforced compensated-shrinkage, quick-setting and hardening, high-ductility cementitious mortar applied at temperatures down to -5°C, with stiff steel fibres for repairing…
Quick-setting and hardening, compensated-shrinkage thixotropic mortar for repairing concrete and fixing drains, manholes and urban fittings in place. TECHNICAL DATA: Maximum dimension of aggregate:…
Quick-setting and hardening, compensated-shrinkage thixotropic mortar for…
Medium-strength (40 MPa), compensated-shrinkage fibre-reinforced thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT T60 with 16.5-17.5 parts…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete.…