One-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: 100 parts of MAPEFER 1K with 20-22 parts of…
One-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
Adhesive zinc plates applied directly on the surface of structures for galvanic cathodic protection against the corrosion of steel reinforcement rods. TECHNICAL DATA: Thickness of plate: 0.25 mm.
Adhesive zinc plates applied directly on the surface of structures for galvanic…
Zinc plate with adhesive backing for galvanic cathodic protection against the corrosion of steel structures exposed to atmospheric conditions. TECHNICAL DATA: Thickness of plate: 0.80 mm. Height: –…
Zinc plate with adhesive backing for galvanic cathodic protection against the…