Two-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: comp. A : comp. B = 3 : 1. Pot life of mix:…
Two-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
One-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: 100 parts of MAPEFER 1K with 20-22 parts of…
One-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
Adhesive zinc plates applied directly on the surface of structures for galvanic cathodic protection against the corrosion of steel reinforcement rods. TECHNICAL DATA: Thickness of plate: 0.25 mm.