Chemical-action vegetable oil-based form-release ready-to-use agent in water emulsion to improve exposed surfaces. Particularly suitable for use on vertical surfaces. Also suitable for steam curing…
Chemical-action vegetable oil-based form-release ready-to-use agent in water…
Chemical-action vegetable oil-based form-release agent in water emulsion to improve exposed surfaces. Particularly suitable for use on horizontal surfaces. Also suitable for steam curing cycles.…
Chemical-action vegetable oil-based form-release agent in water emulsion to…
Polyester, aluminium and epoxy resin metal-effect coloured glitter mixed with used for mixing with KERAPOXY DESIGN. TECHNICAL DATA: Maximum dosage: 10% by weight of KERAPOXY DESIGN. Colours: silver…
Polyester, aluminium and epoxy resin metal-effect coloured glitter mixed with…
Alkali-resistant, primed basalt-fibre mesh for structural “reinforced” strengthening of stone masonry, brick, tuff and concrete surfaces. TECHNICAL DATA: Type of fibre: basalt fibre. Weight: 250…
Alkali-resistant, primed basalt-fibre mesh for structural “reinforced”…
High-strength carbon fibre mesh for “reinforced” structural strengthening work on masonry and concrete structures. TECHNICAL DATA: Type of fibre: high-strength carbon. Weight: ≥170 g/m². Mesh size:…
High-strength carbon fibre mesh for “reinforced” structural strengthening work…
Alkali-resistant, primed glass fibre mesh for structural “reinforced” strengthening of stone, brick and tuff substrates. TECHNICAL DATA: Type of fibre: A.R. type glass fibre. Weight: 225 g/m ² . Mesh…
Alkali-resistant, primed glass fibre mesh for structural “reinforced”…
Fine-grained, fibre-reinforced, normal-setting thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 1 mm. Mixing ratio: 100 parts of MAPEGROUT 430 with 17.5-18.5…
Fine-grained, fibre-reinforced, normal-setting thixotropic mortar for repairing…
Two-component cementitious mortar with a low modulus of elasticity for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT BM comp. A with…
Two-component cementitious mortar with a low modulus of elasticity for…