Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT T60 with 16.5-17.5 parts…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete.…