Two-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: comp. A : comp. B = 3 : 1. Pot life of mix:…
Two-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
Two-component cementitious mortar for finishing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 0.4 mm. Mixing ratio: 4 parts of MAPEFINISH comp. A with 1 part of MAPEFINISH comp. B. Pot…